First time I see cycling data of electrovaya cells in slide 20.
As 3C/3C cycling means 36 charge/discharge cycle/day (1C = full discharge in 1 hour), to achieve 9000 need 250 days, assume to be Litarion present electrode coating (NMP) maybe from Leclanché test (third party data), if we buy idea that non-NMP line will achieve same performance sounds good knowing that 100% discharge is the worst case sounds good.